1.2714 Steel for through hardening

Our selected range provides the right material for any application.

Products

Characteristics

Designation

Strength

max. 250 HB
(≈ max. 850 N/mm²)

Chemical composition

Thermal conductivity at 100 °C

36 W/(mK)

Character

Steel for through hardening, with high-temperature resistance, through hardenability and toughness

Application

Machining

Suited:
EDM, nitriding, etching and hard chrome plating
Polishing: technical polishing possible

Use

Extrusion dies, hot-forging tools, die plates for processing tin, lead and zinc alloys

Heat treatment

Soft annealing:
650 to 700 °C, about 4 to 5 hours
Slow, controlled cooling inside the furnace of 10 to 20 °C per hour to about 600 °C
Further cooling in air, max. 248 HB

Hardening:
950 to 980 °C
Maintain curing temperature for 15 to 30 minutes
Quenching in water/oil
Obtainable hardness: 56 HRC

Tempering:
Slow heating to tempering temperature immediately after hardening
Minimum time in furnace: 1 hour per 20 mm part thickness

Choix boutique

Construction d’outils de découpe
Construction d’outils de découpe
Construction de machines et de gabarits
Construction de machines et de gabarits

Aperçu du panier

Aperçu CAD

Votre panier est vide.
Montant net
Vers le panier